Short answer
For most everyday work PLA and PETG are enough: PLA is the easiest to print, PETG is tougher and handles heat better. For heat and outdoor use look at ABS and ASA, for flexibility TPU, for wear and toughness nylon (PA), for high heat and impact PC, and for stiffness carbon- or glass-fibre filled filaments. Many of these need an enclosure, a hotter nozzle, dry storage or a hardened nozzle, so check your printer can meet those needs before you choose.
Key takeaways
- Choose the material for the part's job; the polymer name alone tells you little.
- PLA and PETG print comfortably on an open printer; ABS, ASA and PA benefit from an enclosure, and PC needs one.
- Nylon and PC absorb moisture quickly and won't print well unless dried and kept dry.
- Carbon- and glass-fibre filled filaments are abrasive; a hardened nozzle is essential.
- Temperatures here are typical ranges; the right value is always in the product's data sheet.
A quick map of filament types
Filaments for FDM printing fall roughly into three groups. First, the everyday materials: PLA, PLA+ and PETG. Second, engineering materials chosen for a specific need: ABS, ASA, TPU, nylon (PA) and PC. Third, composites made by adding fibres to a base polymer: carbon- and glass-fibre filled filaments.
If you're deciding between PLA and PETG, our material selection guide covers that in detail. This post looks at the whole map: when each material makes sense and what it asks of your printer.
Filament comparison chart
| Material | Nozzle °C | Bed °C | Enclosure | Strength | Watch out for |
|---|---|---|---|---|---|
| PLA | 190–220 | 45–60 | Not needed | Easy printing, crisp detail | Low heat resistance, cracks on impact |
| PLA+ | Per maker | Per maker | Not needed | Usually tougher than PLA | No standard definition |
| PETG | 230–250 | 75–90 | Not needed | Tough, better heat and chemical resistance | Stringing, can over-bond to some surfaces |
| ABS | 220–250 | 95–110 | Recommended | Heat resistance, easy to post-process | Warping, odour; ventilation essential |
| ASA | 220–245 | 90–110 | Recommended | UV and outdoor resistance | Warping, odour; ventilation essential |
| TPU | 225–245 | 45–60 | Not needed | Flexibility, shock absorption | Slow printing; direct drive preferred |
| PA (nylon) | 225–265 | 70–90 | Recommended | Toughness, wear resistance | Absorbs moisture very fast; may need an all-metal hotend |
| PC | 260–310 | 80–120 | Required | High heat and impact resistance | All-metal hotend, demanding, moisture |
| CF / GF filled | Per base polymer | Per base polymer | Per base polymer | Stiffness, dimensional stability | Abrasive; hardened nozzle essential |
The most overlooked columns are the two on the right. A material's properties on paper only help if your printer can print it under the right conditions. PC's heat resistance means little while you're trying to print it on a hotend that can't reach 300 °C.
PLA, PLA+ and PETG: the everyday trio
PLA
PLA is the default material for desktop printing. It shrinks little as it cools, often doesn't even need a heated bed, and holds sharp detail well. It likes strong part cooling. Its weakness is heat: it can soften in a car in the sun or next to a warm appliance. It is stiff, but under impact it cracks rather than bends.
PLA is a family in itself. Matte PLA scatters light and hides layer lines; silk PLA gives a glossy, silky surface but is chosen for looks, not strength. Wood- or mineral-filled PLAs offer a different texture, and some wear nozzles faster than usual. “High-speed” PLA is a separate claim, and only means something when backed by measured melt and print data.
PLA+: a label, not a standard
There is no shared definition of PLA+ (or PLA Pro, or Tough PLA). It usually describes a PLA modified with additives that improve impact resistance, but which additive, how much, and how big the difference is all vary between makers. So look past the “PLA+” label to the measured values and test method in the data sheet. It often prints a little hotter than PLA.
PETG
PETG is the bridge between easy printing and real function. It is tougher and more heat-resistant than PLA and still prints on an open printer. In return it tends to string and can bond too strongly to surfaces such as smooth PEI. It is a good default for enclosures, fixtures and parts that will actually be used.
ABS and ASA: heat, outdoor use and ventilation
ABS and ASA are chemical relatives and behave similarly at the printer. Both withstand clearly higher temperatures than PLA; ASA also resists sunlight and weathering, so it replaces ABS for parts that live outdoors.
Their biggest challenge is warping: they shrink as they cool and corners lift off the bed. They need a hot bed, a draught-free space and often an enclosure. Simplify3D recommends an enclosure for ABS; Prusa's material guide treats an enclosure as typically required for ASA too. The general causes of warping are in our troubleshooting guide.
TPU: for flexible parts
TPU is a rubber-like flexible material, ideal for seals, bumpers, grips, vibration dampers and protective cases. Its hardness is usually given on the Shore scale; a lower number means a softer material.
That flexibility makes it harder to print. Pushed, the filament wants to buckle, so a short, tightly constrained path between extruder and hotend matters. Simplify3D recommends direct-drive extruders; in a long Bowden tube TPU can jam. Print slowly, reduce retraction and keep the filament dry.
The hardness you choose affects printing too. A firmer TPU feeds more easily and can print faster; very soft grades need experience and a suitable extruder. For your first TPU, a mid-hardness product is the easy way to learn both the part and the settings. Infill and wall count decide how much a part flexes as much as the material does.
Nylon (PA) and PC: the engineering end
Nylon is known for toughness and wear resistance: gears, hinges, sliding parts. Its biggest challenge is moisture. PA takes on moisture from the air very fast, and damp nylon gives bubbly, weak, rough parts. Expect poor results unless you dry it and feed it from a dry box throughout the print; the principles are in our storage and drying guide.
PC (polycarbonate) is for parts that need high heat and impact resistance. Its typical nozzle range of 260 to 310 °C means an all-metal hotend, and Simplify3D lists an enclosure as required. It is prone to warping and oozing and absorbs moisture too. In return it makes parts that work where other desktop materials give up.
With both materials, the number on paper and the printed part can differ. Layer bonding, print orientation and moisture content all change the result noticeably. For a critical part, don't decide without testing in real conditions.
Carbon- and glass-fibre filled filaments
Carbon-fibre (CF) and glass-fibre (GF) filled filaments are made by adding short chopped fibres to a base polymer such as PLA, PETG, PA or PC. The fibres make parts stiffer and can improve dimensional stability by reducing shrinkage as the part cools. The surface is usually matte, with less visible layer lines.
- Nozzle: the fibres are abrasive. A standard brass nozzle wears out quickly; hardened steel or a similar wear-resistant nozzle is essential.
- Base polymer: print temperature, enclosure and moisture needs come from the base. CF-PLA prints much like PLA; CF-PA brings all of nylon's challenges.
- Brittleness: stiffer doesn't mean tougher. Fibre-filled parts can break more easily on impact than the unfilled base polymer.
- Direction: fibres align with the print path, so the part is strong in one direction and weaker between layers.
Which filament for which job
| What the part does | First choice | Alternative |
|---|---|---|
| Visual prototype, model, figurine | PLA | Matte or silk PLA |
| Functional prototype, enclosure, fixture | PETG | ABS, ASA |
| Outdoors, in the sun | ASA | PETG (short term) |
| Warm environment, inside a device | ABS, PC | PA |
| Flexible part, seal, bumper | TPU | TPU in another hardness |
| Gear, hinge, wearing part | PA | CF-PA |
| Stiff fixture, bracket | CF or GF filled | PETG, PA |
If you're unsure, print the same part in two materials and test it in real conditions. Whichever material you pick, the spool itself matters too: see our filament quality checklist for diameter consistency, moisture and winding.
At AMENT, the launch focus is the Core family: PLA and PETG. ASA, TPU, PA, PC and carbon- and glass-fibre filled materials sit in the planned Pro family, each with its own requirements and limits. None of them is on sale yet and no measured data has been published; you can see the plan on the materials page.
When you switch materials
- Purge the nozzle: going from a high-temperature material to PLA, push the old material through fully at the higher temperature, then lower it.
- Check the surface: not every material likes every build plate; PETG can over-bond to some, while ABS and ASA want a hotter bed.
- Dry it: before switching to nylon, PC or TPU, dry the filament and feed it from a dry box.
- Change the profile: temperature, cooling, retraction and speed are material-specific. For the calibration order with a new material, see the print settings guide.
Frequently asked questions
What is the best filament for beginners?
For most people, PLA. It prints at low temperatures, shrinks little, works without trouble even on an open printer and holds detail well. If your part will face heat or impact, the usual next step is PETG.
What is the difference between PLA and PLA+?
There is no common standard for PLA+. It usually means a PLA modified with additives to improve impact resistance, but the content and the size of the difference vary by maker. Look at the measured values and test method in the data sheet, not the label.
What is the difference between ABS and ASA?
Both print similarly and resist heat better than PLA. ASA also resists sunlight and weathering, so it is preferred for parts that stay outdoors. Both tend to warp, benefit from an enclosure and need good ventilation.
Do I need a special nozzle for carbon fibre filament?
Yes. Carbon and glass fibre are abrasive and wear a standard brass nozzle quickly. Use hardened steel or another wear-resistant nozzle. Temperature and enclosure needs depend on the base polymer.
Which filaments need an enclosed printer?
PLA, PETG and TPU usually print on an open printer. ABS, ASA and nylon benefit clearly from an enclosure, and PC generally needs one. An enclosure does not replace ventilation.
Sources
- 1Simplify3D Materials Guide: PLA
- 2Simplify3D Materials Guide: PETG
- 3Simplify3D Materials Guide: ABS
- 4Simplify3D Materials Guide: ASA
- 5Simplify3D Materials Guide: Flexible (TPE/TPU)
- 6Simplify3D Materials Guide: Nylon
- 7Simplify3D Materials Guide: Polycarbonate
- 8Simplify3D Materials Guide: Carbon Fiber Filled
- 9Filament Material Guide (Prusa Knowledge Base)
- 10Azimi et al.: Emissions of Ultrafine Particles and Volatile Organic Compounds from Commercially Available Desktop 3D Printers with Multiple Filaments (Environmental Science & Technology, 2016)